ASTM D3802 Standard Test Method for Ball-Pan Hardness of Activated Carbon
Данный раздел/документ содержится в продуктах:
- Техэксперт: Машиностроительный комплекс
- Картотека зарубежных и международных стандартов
- ASTM F1412 Standard Specification for Polyolefin Pipe and Fittings for Corrosive Waste Drainage Systems
- 23
- ASTM F1412 Standard Specification for Polyolefin Pipe and Fittings for Corrosive Waste Drainage Systems
- 23.040
- ASTM F1412 Standard Specification for Polyolefin Pipe and Fittings for Corrosive Waste Drainage Systems
- 23.040.20
- ASME B16.21 Nonmetallic Flat Gaskets for Pipe Flanges
- ASTM F363 Standard Test Method for Corrosion Testing of Gaskets
- ASTM F112 Standard Test Method for Sealability of Enveloped Gaskets
- ASTM F363 Standard Test Method for Corrosion Testing of Gaskets
- ASTM F363 Standard Test Method for Corrosion Testing of Gaskets
- ASTM F112 Standard Test Method for Sealability of Enveloped Gaskets
- ASTM F112 Standard Test Method for Sealability of Enveloped Gaskets
- ASTM F336 Standard Practice for Design and Construction of Nonmetallic Enveloped Gaskets for Corrosive Service
- ASTM B280 Standard Specification for Seamless Copper Tube for Air Conditioning and Refrigeration Field Service
- ASME AG-1 Code on Nuclear Air and Gas Treatment
- Картотека зарубежных и международных стандартов
ASTM International
Standard Test Method for Ball-Pan Hardness of Activated Carbon
N D3802
Annotation
This test method covers a procedure for determining the ball-pan hardness number of granular activated carbons. For the purpose of this test, granular activated carbons are those having particles 90 % of which are larger than 80 mesh (180 ?m) as determined by Test Method D2862.
The values stated in SI units are to be regarded as standard. No other units of measurement are included in this standard.
This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.
Автоматический перевод:
Стандартный метод испытаний для твердости поддона шара активированного угля
Этот метод тестирования покрывает процедуру для определения количества твердости панорамирования шара гранулированного активированного угля. В целях этого теста гранулированный активированный уголь - те, которые имеют частицы, 90% которых больше, чем 80 сеток (180 m), как определено Методом тестирования D2862.
Значения, утвержденные в единицах СИ, должны рассматриваться как стандарт. Никакие другие единицы измерения не включены в этот стандарт.