BSI BS 3473-5 Chemical Resistance of Glass Used in the Production of Laboratory Glassware Part 5: Method for Determination of Resistance of Glass to Attack by 6 mol/L Hydrochloric Acid at 100 Degrees C
Данный раздел/документ содержится в продуктах:
- Техэксперт: Машиностроительный комплекс
- Картотека зарубежных и международных стандартов
- BSI BS 3473-1 Chemical Resistance of Glass Used in the Production of Laboratory Glassware Part 1: Method for Determination of Resistance of Glass to Attack by a Boiling Aqueous Solution of Mixed Alkali
- 81
- BSI BS 3473-1 Chemical Resistance of Glass Used in the Production of Laboratory Glassware Part 1: Method for Determination of Resistance of Glass to Attack by a Boiling Aqueous Solution of Mixed Alkali
- 81.040
- BSI BS 3473-1 Chemical Resistance of Glass Used in the Production of Laboratory Glassware Part 1: Method for Determination of Resistance of Glass to Attack by a Boiling Aqueous Solution of Mixed Alkali
- 81.040.01
- BSI BS 3473-1 Chemical Resistance of Glass Used in the Production of Laboratory Glassware Part 1: Method for Determination of Resistance of Glass to Attack by a Boiling Aqueous Solution of Mixed Alkali
- BSI BS 3473-3 Chemical Resistance of Glass Used in the Production of Laboratory Glassware Part 3: Method for Determination of Hydrolytic Resistance of Glass Grains at 121 Degrees Centigrade
- BSI BS 3473-3 Chemical Resistance of Glass Used in the Production of Laboratory Glassware Part 3: Method for Determination of Hydrolytic Resistance of Glass Grains at 121 Degrees Centigrade
- BSI BS 5732 Specification for Glass disposable Pasteur pipettes
- BSI BS 3473-2 Chemical Resistance of Glass Used in the Production of Laboratory Glassware Part 2: Method for Determination of Hydrolytic Resistance of Glass Grains at 98 Degrees Centigrade
- Картотека зарубежных и международных стандартов
British Standards Institution
Chemical Resistance of Glass Used in the Production of Laboratory Glassware Part 5: Method for Determination of Resistance of Glass to Attack by 6 mol/L Hydrochloric Acid at 100 Degrees C
N BS 3473-5
Annotation
Methods for determining and classifying the amount of alkali metal oxides released from the surface of glassware when subject to attack at 100 ± 1°C for 3 h.
Автоматический перевод:
Химическая стойкость Стекла, Используемого в Производстве Лабораторной Части 5 Стеклянной посуды: Метод для Определения Устойчивости к Стеклу для Нападения 6 mol/L Соляными кислотами в 100 градусах по Цельсию
Методы для определения и классификации суммы оксидов щелочного металла выпустили от поверхности стеклянной посуды когда подвергающийся для нападения в 100 ± 1°C в течение 3 ч.
Эквиваленты данного стандарта: