ASTM D3402/D3402M Standard Test Method for Tumbler Test for Coke
Данный раздел/документ содержится в продуктах:
- Техэксперт: Машиностроительный комплекс
- Картотека зарубежных и международных стандартов
- ASTM F1412 Standard Specification for Polyolefin Pipe and Fittings for Corrosive Waste Drainage Systems
- 23
- ASTM F441/F441M Standard Specification for Chlorinated Poly(Vinyl Chloride) (CPVC) Plastic Pipe, Schedules 40 and 80
- ASTM D1785 Standard Specification for Poly(Vinyl Chloride) (PVC) Plastic Pipe, Schedules 40, 80, and 120
- ASTM F480 Standard Specification for Thermoplastic Well Casing Pipe and Couplings Made in Standard Dimension Ratios (SDR), SCH 40 and SCH 80
- ASTM D1785 Standard Specification for Poly(Vinyl Chloride) (PVC) Plastic Pipe, Schedules 40, 80, and 120
- ASTM D1785 Standard Specification for Poly(Vinyl Chloride) (PVC) Plastic Pipe, Schedules 40, 80, and 120
- ASTM F480 Standard Specification for Thermoplastic Well Casing Pipe and Couplings Made in Standard Dimension Ratios (SDR), SCH 40 and SCH 80
- ASTM F480 Standard Specification for Thermoplastic Well Casing Pipe and Couplings Made in Standard Dimension Ratios (SDR), SCH 40 and SCH 80
- ASTM D2122 Standard Test Method for Determining Dimensions of Thermoplastic Pipe and Fittings
- ASTM F2390 Standard Specification for Poly(Vinyl Chloride) (PVC) Plastic Drain, Waste, and Vent (DWV) Pipe and Fittings Having Post-Industrial Recycle Content
- ASTM D2774 Standard Practice for Underground Installation of Thermoplastic Pressure Piping
- ASTM E11 Standard Specification for Woven Wire Test Sieve Cloth and Test Sieves
- Картотека зарубежных и международных стандартов
ASTM International
Standard Test Method for Tumbler Test for Coke
N D3402/D3402M
Annotation
This test method describes a procedure for obtaining a relative measure of the resistance to degradation of coke by impact and abrasion.
Standard Procedure—This procedure uses a coke sample sized to ?75 mm [?3 in.] and + 50 mm [ + 2 in.].
Alternative Procedure—This procedure using coke sized 50% of 63 by 50 mm [21?2 by 2 in.] and 50 % of 50 by 37.5 mm [2 by 11?2 in.].
The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in non-conformance with the standard.
This standard does not purport to address all of the safety problems, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.
Автоматический перевод:
Стандартный метод испытаний для испытания стакана на кока-колу
Этот метод тестирования описывает процедуру для получения относительной меры сопротивления ухудшению кокса влиянием и стиранием.
Стандартная процедура — Эта процедура использует коксовый образец, измеренный для 75 мм [ 3 в.] и + 50 мм [+ 2 дюйма.].