ASTM A959 Standard Guide for Specifying Harmonized Standard Grade Compositions for Wrought Stainless Steels
Данный раздел/документ содержится в продуктах:
- Техэксперт: Машиностроительный комплекс
- Картотека зарубежных и международных стандартов
- ASTM A1082/A1082M Standard Specification for High Strength Precipitation Hardening and Duplex Stainless Steel Bolting for Special Purpose Applications
- ASTM A959 Standard Guide for Specifying Harmonized Standard Grade Compositions for Wrought Stainless Steels
- ASTM F2080 Standard Specification for Cold-Expansion Fittings With Metal Compression-Sleeves for Cross-Linked Polyethylene (PEX) Pipe
- 23
- ASTM F2080 Standard Specification for Cold-Expansion Fittings With Metal Compression-Sleeves for Cross-Linked Polyethylene (PEX) Pipe
- 23.040
- ISO 21049 Pumps Shaft sealing systems for centrifugal and rotary pumps - First Edition
- ASME B73.2 Specification for Vertical In-Line Centrifugal Pumps for Chemical Process
- ASTM A519 Standard Specification for Seamless Carbon and Alloy Steel Mechanical Tubing
- ASTM A1040 Standard Guide for Specifying Harmonized Standard Grade Compositions for Wrought Carbon, Low-Alloy, and Alloy Steels
- Картотека зарубежных и международных стандартов
ASTM International
Standard Guide for Specifying Harmonized Standard Grade Compositions for Wrought Stainless Steels
N A959
Annotation
This guide provides a guide to ASTM Subcommittees A01.06, A01.10, A01.17, A01.22, and A01.28 for specifying chemical composition limits of wrought stainless steels. It is intended that these recommended grade composition limits be suitable for adoption by other standardization bodies that prepare standards for stainless steel products
Included in this guide are the recommendations for determining the number of significant figures for specifying chemical composition from Test Methods, Practices, and Terminology A751
All stainless steel UNS numbers and the stainless steel grades in all standards overseen by the aforementioned ASTM subcommittees have been included, except those grades applicable to restricted special end uses and alloys containing less than 10.5 % minimum chromium
Not addressed are minor composition modifications which a specific product subcommittee may find necessary to accommodate effects of normal processing or to enhance fabricability by the producer or user, or both
Also not generally addressed (except when established byASTM product subcommittees) is a complete rationalization of all limits, especially when such would conflict with longstanding practices and is not justified by special technical effect
Excluded from this guide are cast material and welding filler metal