CEN EN ISO 13934-1 Textiles - Tensile Properties of Fabrics - Part 1: Determination of Maximum Force and Elongation at Maximum Force Using the Strip Method
Данный раздел/документ содержится в продуктах:
- Техэксперт: Машиностроительный комплекс
- Картотека зарубежных и международных стандартов
- CEN EN ISO 11721-1 Textiles - Determination of the Resistance of Cellulose-Containing Textiles to Micro-Organisms - Soil Burial Test - Part 1: Assessment of Rot-Retardant Finishing
- 07
- CEN EN ISO 11721-1 Textiles - Determination of the Resistance of Cellulose-Containing Textiles to Micro-Organisms - Soil Burial Test - Part 1: Assessment of Rot-Retardant Finishing
- 07.100
- CEN EN ISO 11721-1 Textiles - Determination of the Resistance of Cellulose-Containing Textiles to Micro-Organisms - Soil Burial Test - Part 1: Assessment of Rot-Retardant Finishing
- 07.100.99
- 59
- CEN EN ISO 11721-1 Textiles - Determination of the Resistance of Cellulose-Containing Textiles to Micro-Organisms - Soil Burial Test - Part 1: Assessment of Rot-Retardant Finishing
- 59.080
- BSI BS EN ISO 11721-2 Textiles Determination of the resistance of cellulose-containing textiles to micro-organisms Soil burial test Part 2: Identification of long-term resistance of a rot retardant finish
- Картотека зарубежных и международных стандартов
European Committee for Standardization
Textiles - Tensile Properties of Fabrics - Part 1: Determination of Maximum Force and Elongation at Maximum Force Using the Strip Method
N EN ISO 13934-1
Annotation
This part of ISO 13934 specifies a procedure to determine the maximum force and elongation at maximum force of textile fabrics using a strip method.
NOTE ISO 13934-2 describes the method known as the grab method. For informative reference, see Bibliography
The method is mainly applicable to woven textile fabrics, including fabrics which exhibit stretch characteristics imparted by the presence of an elastomeric fibre, mechanical, or chemical treatment. It can be applicable to fabrics produced by other techniques. It is not normally applicable to geotextiles, nonwovens, coated fabrics, textile-glass woven fabrics, and fabrics made from carbon fibres or polyolefin tape yarns (see Bibliography).
The method specifies the determination of the maximum force and elongation at maximum force of test specimens in equilibrium with the standard atmosphere for testing, and of test specimens in the wet state.
The method is restricted to the use of constant rate of extension (CRE) testing machines.