ASTM D876 Standard Test Methods for Nonrigid Vinyl Chloride Polymer Tubing Used for Electrical Insulation

Список продуктов
Данный раздел/документ содержится в продуктах:

 

ASTM International

Standard Test Methods for Nonrigid Vinyl Chloride Polymer Tubing Used for Electrical Insulation
 N D876

 

Annotation

 

These test methods cover the testing of general-purpose (Grade A), low-temperature (Grade B), and high-temperature (Grade C)2 nonrigid vinyl chloride polymer tubing, or its copolymers with other materials, for use as electrical insulation. For the purpose of these test methods nonrigid tubing shall be tubing having an initial elongation in excess of 100 % at break.

NOTE 1—These test methods are similar but not identical to those in IEC 60684–2.

The values stated in inch-pound units are to be regarded as standard, except for temperature, which shall be expressed in degrees Celsius. The values given in parentheses are mathematical conversions to SI units that are provided for information only and are not considered standard.

*A Summary of Changes section appears at the end of this standard

2 Test methods applicable to Grade B will be specified at a later date.

 

Автоматический перевод:

 

Методы стандартной пробы для нетвердого шланга трубки полимера винилхлорида, используемого для электрической изоляции

Эти методы тестирования покрывают тестирование общего назначения (Класс A), низкая температура (Класс B), и высокотемпературный (Класс C) 2 нетвердых виниловых трубки полимера хлорида или ее сополимеры с другими материалами, для использования в качестве электрической изоляции. В целях этих методов тестирования нетвердая трубка должна быть трубкой, имеющей начальное удлинение сверх 100% в повреждении.

Категории продуктов

 

 

 

Знакомьтесь, "Техэксперт"

 Техэксперт для iPad

 Для Android

АКЦИЯ!

Бесплатный доступ