ASTM D3681 Standard Test Method for Chemical Resistance of “Fiberglass” (Glass–Fiber–Reinforced Thermosetting-Resin) Pipe in a Deflected Condition
Данный раздел/документ содержится в продуктах:
- Техэксперт: Машиностроительный комплекс
- Картотека зарубежных и международных стандартов
- ASTM F1412 Standard Specification for Polyolefin Pipe and Fittings for Corrosive Waste Drainage Systems
- 23
- ASTM F1412 Standard Specification for Polyolefin Pipe and Fittings for Corrosive Waste Drainage Systems
- 23.040
- ASME B31E Standard for the Seismic Design and Retrofit of Above-Ground Piping Systems
- ASME B16.21 Nonmetallic Flat Gaskets for Pipe Flanges
- ASTM F363 Standard Test Method for Corrosion Testing of Gaskets
- ASTM F112 Standard Test Method for Sealability of Enveloped Gaskets
- ASTM F336 Standard Practice for Design and Construction of Nonmetallic Enveloped Gaskets for Corrosive Service
- ISO FDIS 24817 Petroleum, petrochemical and natural gas industries - Composite repairs for pipework - Qualification and design, installation, testing and inspection
- Картотека зарубежных и международных стандартов
ASTM International
Standard Test Method for Chemical Resistance of “Fiberglass” (Glass–Fiber–Reinforced Thermosetting-Resin) Pipe in a Deflected Condition
N D3681
Annotation
This test method covers the procedure for determining the chemical-resistant properties of fiberglass pipe in a deflected condition for diameters 4 in. (102 mm) and larger. Both glass–fiber–reinforced thermosetting resin pipe (RTRP) and glass–fiber–reinforced polymer mortar pipe (RPMP) are fiberglass pipes.
NOTE 1 - For the purposes for this standard, polymer does not include natural polymers.
Inch-pound units are to be regarded as the standard. The values given in parentheses are for information only.
This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. Specific precautionary statements are given in 9.5.
NOTE 2 - There is no known ISO equivalent to this standard.
Автоматический перевод:
Стандартный метод испытаний для химической стойкости “стекловолокна” (укрепленная стекловолокном термореактивная смола) труба в отклоненном условии
Этот метод испытаний покрывает процедуру для определения химически-стойких свойств стекловолоконной трубы в отклоненном условии для диаметров 4 дюйма. (102 мм) и больше. И укрепленная стекловолокном труба термореактивной смолы (RTRP) и укрепленная стекловолокном полимерная труба миномета (RPMP) являются стекловолоконными трубами.